I am currently doing some induction seal liner testing on acidic based chemical and things are touch and go
We are testing Selig FS 1-19 liners (not having success) and Selib SG75M liners (success we are weary). Both of these were sealed at 65 heat and 1.2 second dwell time
Does anybody have any thoughts on this? Has anyone had success with another liner? Perhaps settings need to be altered?
------------------------------